Material |
Cutting Speed V (m/min) |
Feed Rate (mm/rev) |
Coolant |
| |
|
4 mm |
6 mm |
10 mm |
16 mm |
20 mm |
|
Low alloy Steel upto 900N/mm2 Over 700N/mm2 |
12-15 12-15 |
0.12 0.1
|
0.16 0.12
|
0.2 0.16 |
0.25 0.2 |
0.35 0.3
|
Soluble oil |
High Alloy Steels upto 900N/mm2 upto 1250N/mm2 upto 1250N/mm2
|
10-15 8-12 6-10 |
0.12 0.1 0.08 |
0.16 0.12 0.1
|
0.2 0.16 0.12 |
0.25 0.2 0.16 |
0.3 0.25 0.2
|
Soluble oil |
| Cr-Ni alloyed steels |
8-10 |
0.08
|
0.1
|
0.12 |
0.16 |
0.2 |
Cutting Oil |
Gray Cast Iron up to 200 Brinell Over to 200 Brinell |
12-15 8-12 |
0.12 0.1 |
0.16 0.12 |
0.2 0.16 |
0.25 0.2 |
0.35 0.3 |
Dry Soluble Oil |
Malleable Cast Iron upto 450 N/mm2 |
8-12 |
0.1 |
0.12 |
0.16 |
0.2 |
0.3 |
Soluble oil |
Copper Industrial Electrolytic |
15-30 15-20 |
0.14 0.1 |
0.2 0.12 |
0.25 0.16 |
0.3 0.2
|
0.35 0.25 |
Soluble oil |
Aluminum Soft long chipping with up to 12% Si with Over to 12% Si
|
15-30 15-30 10-20 |
0.14 0.12 0.1 |
0.2 0.16 0.12 |
0.25 0.2 0.16 |
0.3 0.25 0.2 |
0.4 0.35 0.25 |
Soluble oil Soluble oil |