Material |
Type |
VC (m/min) |
Feed Rate f/tooth |
Coating |
Coolant |
| Low alloy Steel upto |
Standard Length |
120 |
0.05 |
TiAlN/TiN |
Soluble |
| 700N/mm 2 |
Long |
90 |
0.04 |
TiAlN/TiN |
Soluble |
| High Alloy steels upto |
Standard Length |
120 |
0.04 |
TiAlN/TiN |
Soluble |
| 900N/mm 2 |
Long |
90 |
0.03 |
TiAlN/TiN |
Soluble |
| High Alloy steels above |
Standard Length |
100 |
0.03 |
TiAlN/TiN |
Soluble |
| 900N/mm 2 |
Long |
80 |
0.02 |
TiAlN/TiN |
Soluble |
| Tool Steel/Ball Bearing |
Standard Length |
60 - 100 |
0.02 |
TiAlN/TiN |
Soluble |
| steel |
Long |
60-100 |
0.02 |
TiAlN/TiN |
Soluble |
Stainless/Heat resistance
|
Standard Length |
45 -60 |
0.02 |
TiAlN |
Oil |
| steel |
Long |
40-50 |
0.01 |
TiAlN |
Oil |
| Gray Cast Iron |
Standard Length |
120-140 |
0.05 |
TiAlN |
Soluble/Mist |
| |
Long |
90 - 120 |
0.04 |
TiAlN |
Soluble/Mist |
| Malleable Cast Iron |
Standard Length |
120-140 |
0.05 |
TiAlN |
Soluble/Mist |
| |
Long |
90 - 120 |
0.04 |
TiAlN |
Soluble/Mist |
| Brass/German Silver |
Standard Length |
200 - 250 |
0.06 |
TiN |
Air/Mist |
| |
Long |
150 - 200 |
0.05 |
TiN |
Air/Mist |
| Aluminum |
Standard Length |
250 - 400 |
0.06 |
TiN |
Soluble |
Rolled/Cast/alloys with upto 10% Si |
Long |
250 - 400 |
0.06 |
TiN |
Soluble |
| Aluminum |
Standard Length |
250 - 400 |
0.06 |
TiN |
Soluble |
Rolled/Cast/alloys with upto 10% Si |
Long |
250 - 400 |
0.06 |
TiN |
Soluble |
Note : Cutting speed & feed rate are given only for guidance purpose. It is to be established in application.